Causes of rusting of 20# precision steel pipe and prevention methods

1. The surface of the stainless steel accumulates dust or other metal particles attached to other metal elements. In humid air, the condensed water between the attached material and the stainless steel connects the two into a micro battery, triggering an electrochemical reaction. The protective film is damaged and is called electrochemical corrosion.
2. The surface of the stainless steel adheres to the organic juice, which forms an organic acid in the presence of water and oxygen, and forms an organic acid to corrode the metal surface for a long time.
3. The surface of the stainless steel adheres to acid, alkali, and salt substances (such as alkaline water and lime water sprayed on the wall) to cause local corrosion.
4. In the polluted air (the atmosphere containing a large amount of sulfides, oxides, hydrogen oxide), in the case of condensed water, sulfuric acid, nitric acid, acetic acid liquid spots are formed, causing chemical corrosion.

All of the above can cause damage to the stainless steel surface protective film and cause corrosion. Therefore, in order to ensure that the metal surface is permanently bright and not rusted, we recommend:
1. For the 20# precision steel pipe in transportation. Some trucks have rust inside the compartment. If it is not sure whether the packaging bag of the pipe is worn during loading and unloading, then the car should be placed on the bottom layer to place some wood or wood, etc., to separate the pipe from the floor of the car.

2. When the pipe is stacked, pay attention to it. Try to find a place that is clean and ventilated. Especially when the materials purchased by the engineering customer are placed on the site, avoid placing it with other volatile materials to reduce the permeability of the acid-alkaline gas to the surface of the pipe. 

3. When using the pipe, the worker should work with gloves as much as possible. The soaking of sweat also affects the 20# precision steel pipe.



New service from OilVoice
Trip Shepherd is for companies who need to track their staff in areas of risk.
It's free to use, so we invite you to try it.

Visit source site

https://permanentsteel.com/product/stainless-steel...

20 precision steel pipepreventive measuresruststainless steel

More items from lvy


How to Maintain Oil Casing Pipe

At present, many oil companies are protecting oil casing pipe , and do not allow the use of wear-resistant belts. So how to repair the casing problem? Many drilling companies have tried many methods to remove the toughness of the tungsten carbide of the drill pipe. In the welding process of the wea ...

lvy lee - Permanent Steel Manufacturing Co.,Ltd


Posted 9 days agoPress > casing pipeOil and GasMaintain

Types of Oil Casing and Their Respective Uses

According to the function of casing pipe , it can be divided into surface casing, technical casing and oil casing. 1) Surface casing of petroleum casing: 1. It is used to block the unstable and soft, easily collapsed and leaking stratum and water layer in the upper part; 2. Install a wellhead devic ...

lvy lee - Permanent Steel Manufacturing Co.,Ltd


Posted 9 days agoPress > casing pipecasing typecasing uses

The Technological Development Process of ERW Steel Pipes at Home and Abroad

High frequency straight seam welded pipe (ERW) is the hot rolled coil plate formed by the forming machine, using the skin effect and proximity effect of high frequency current to heat and melt the edge of the tube blank, and pressure welding under the action of the squeeze roller To achieve product ...

lvy lee - Permanent Steel Manufacturing Co.,Ltd


Posted 16 days agoPress > erw steel pipeTechnological DevelopmentHome and Abroad +1

Corrosion Mechanism and Anti-corrosion Process of Oil Well Casing

The damage to the wellbore structure of oil fields and water wells not only affects the normal production of damaged wells, but also affects the normal development of adjacent wells and even blocks, and poses a great threat to the stable production of the entire oil field. The main factors that caus ...

lvy lee - Permanent Steel Manufacturing Co.,Ltd


Posted 16 days agoPress > well casingAnti-corrosion ProcessCorrosion Mechanism +1

Anti-corrosion Process of Oil Casing Pipe

Corrosion of oil casing is related to factors such as partial pressure of corrosive gas, ambient temperature, water content, salinity, flow rate, pH value and so on. So what are the anti-corrosion processes of the oil  casing pipe ? Let 's take a brief look: 1. Cement sealing anticorrosion skills I ...

lvy lee - Permanent Steel Manufacturing Co.,Ltd


Posted 19 days agoPress > casing pipeAnti-corrosion Processmining industry
All posts from lvy